RESIN PUROLITE MB478LT

 

 

Purolite MB 478LT is ready-for-use, uniformly mixed bed, intended for the production of demineralized water of high purity. It is especially recommended for spark erosion machines where, due to good kinetics of exchange, it can obtain good results due to assuring the correct specific resistance of circulation water for long periods of time.
Purolite MB 478LT is prepared by thorough mixing of two fully regenerated ion-exchange resins having gel structure – strong acidic cationite and strong basic anionite of type I.

Material Safety data Sheet

 

 

 

    Table 1 – Typical physical and Chemical properties

Physical aspect Spherical grains
Functional groups Sulfonic acid and quaternary ammonium
Ionic form (at dispatch) H+/OH-
Cationite to anionite resin ratio 1.0/1.0
Range of particle size 0.3 – 1.2 mm
Humidity ~ 60 %
Bulk density 700 – 750 g/l
Standard package 25-litre bags
Recommended flow speed 10 – 50 OZ/h
Working volume
(end point at 10 μS/cm)
30 g CaCO3/l
Average conductivity
of treated water
1.0 – 5.0 mS/cm
pH of treated water 6.0 – 7.0

  NOTE:: The product should be stored in original bags or other appropriate and sealed containers. The resin should not lose its humidity and should not be exposed to air. Its transfer to the working column should be performed in a wet state or when submerged in water.

 

Privacy Overview

This website uses cookies, which enables the use of cookies. The cookies that are categorized as necessary are used based on the basic functionality of the functionality. We also use cookies that are used to analyze and understand how you use this website. These cookies can only be used in your application using this tool. You also have the option to allow these cookies. However, opting out of some of these cookies may be available for your browsing experience.